Static Compressive Creep
  • Average strain (deformation under load) exhibited by PMMA after 25 hours was 10 times greater than that exhibited by Cortoss®
  • Cortoss® strain at 25 hours:
    • 2.2% at 50 MPa
  • PMMA strain at 25 hours
    • 23% at 50 MPa
Static Compressive Creep
  • More than twice the mean static compressive strength of PMMA, as determined in testing and as reported in the medical literature
    • 211.0 vs 94.9, respectively
    • Cortoss® mean static compressive strength is most like cortical bone (20 MPa)